Item | gas pressure sintering | hot pressing sintering | reactive sintering | pressureless sintering |
Rockwell hardness | ≥75HRA | - | >80HRA | 91-92HRA |
Volume density | 3.25g/cm3 | >3.25g/cm3 | 1.8-2.7g/cm3 | 3.0-3.2 g/cm3 |
Dielectric constant | - | 8.0( @ 20℃, 1 MHz) | - | - |
electric volume resistivity | 10^14 Ω·cm | 10^8Ω·cm | - | - |
breaking tenacity | 6-9 MPa·m¹/² | 6-8MPa·m¹/² | 2.8MPa·m¹/² | 5-6MPa·m¹/² |
Elasticity modulus | 300-320GPa | 300-320GPa | 160-200GPa | 290-320GPa |
thermal expansivity | 3.1-3.3m/K ×10^-6 /℃ | 3.4m/K×10^-6 /℃ | 2.53m/K×10^-6 /℃ | 600m/K×10^-6 /℃ |
thermal conductivity | 15-20W/(m·K) | 34W/(m·K) | 15W/(m·K) | - |
weibull modulus | 12-15 | 15-20 | 15-20 | 10-18 |
Note:The above data is only for your reference. | ||||